Stable free radical polymerization process and thermoplastic materials produced therefrom
US5449724A · kind A · utility
45Cited by
15References
17Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Dec 14, 1994 |
| Grant date | Sep 12, 1995 |
| Priority date | — |
| Expiry date | Dec 14, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F10/02
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A free radical polymerization process for the preparation of a thermoplastic resin includes heating a mixture comprised of a free radical initiator, a stable free radical agent, and ethylene at a temperature of from about 40.degree. C. to about 500.degree. C. and at a pressure of from about 500 to about 5,000 bar to form a thermoplastic resin. The thermoplastic resin has a molecular weight distribution of from about 1.0 to about 2.0.