Patent · US Expired

Method for preparing refined kaolin in clay products

US5454865A · kind A · utility

24Cited by
13References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 23, 1993
Grant dateOct 3, 1995
Priority date
Expiry dateDec 23, 2013

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/60
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A method which enables economical and highly effective preparation of refined kaolin clay products having preselected particle size distributions and brightnesses, by means of separate, efficient and economical processing of at least two crude components. A fine particle size kaolin crude having a PSD such that at least 85% by weight of the particles are of less than 2 micrometers ESD is wet beneficiated to provide a first product component having a PSD of at least 95% by weight less than 2 micrometers and a brightness of at least 89 on the G.E. scale. This wet beneficiation is conducted without use of a froth flotation step. A coarse particle size kaolin crude having a PSD such that less than 85% by weight of particles are of less than 2 micrometers ESD, is separately wet beneficiated to produce a second product component having a PSD of no more than 85% by weight less than 2 micrometers and a brightness of at least 89 on the G.E. scale. This last wet beneficiation is, however, conducted with use of a conventional froth flotation step. The first and second product components are then blended in proportions to produce the desired refined kaolin clay product having a preselected PSD…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.