Tin oxide filled dimethylsiloxane-fluoroalkylsiloxane fuser roll for fixing toner to a substrate
US5464703A · kind A · utility
41Cited by
14References
20Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 29, 1994 |
| Grant date | Nov 7, 1995 |
| Priority date | — |
| Expiry date | Jun 29, 2014 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31678
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A fuser member useful for heat-fixing an electrographic toner to a substrate, a composition of matter and a preparation method. The fuser member has a core and a base cushion layer overlying the core. The base cushion layer includes a crosslinked poly(dimethylsiloxane-fluoroalkylsiloxane) elastomer that has tin oxide particles dispersed therein in a concentration of from 20 to 40 percent of the total volume of the base cushion layer.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.