Process for preparing high-molecular weight polyesters
US5468441A · kind A · utility
2Cited by
1References
14Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Aug 22, 1994 |
| Grant date | Nov 21, 1995 |
| Priority date | — |
| Expiry date | Aug 22, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G63/54
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A high-molecular-weight polyester is prepared by polycondensing an aromatic dicarboxylic acid with a mixture of alkanediols and alkenediols with substantial exclusion of oxygen and in the presence of a catalyst, until a viscosity number in the range from 50 to 140 cm.sup.3 /g is reached and then postcondensing the polycondensed material in the solid-phase until the required viscosity number is reached.