Production of blow molding polyethylene resin
US5473027A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 9, 1994 |
| Grant date | Dec 5, 1995 |
| Priority date | — |
| Expiry date | Jun 9, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F10/02
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Disclosed is a process for making polyethylene resin by reacting ethylene or ethylene and a C.sub.3 -C.sub.8 alpha-olefin in the presence of a CrO.sub.3 /TiO.sub.2 catalyst on a silica support in a gas-phase polymerization reactor and in the presence of a catalyst productivity reduction agent such as oxygen. The resin in one embodiment has a melt flow ratio between 65 and 140 and a melt index between 0.1 and 0.6 g/10 min. The resin is particularly suitable for use in blow-molding applications.