Aluminum base alloy

US5484493A · kind A · utility

5Cited by
7References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 27, 1995
Grant dateJan 16, 1996
Priority date
Expiry dateJan 27, 2015

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C1/026
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Aluminum base alloy consisting essentially of from 0.1 to 3.0% boron, from 1 to 10% titanium and the balance essentially aluminum wherein the aluminum matrix contains TiB.sub.2 particles dispersed throughout said matrix having an average particle size of less than 1 micron, and wherein the matrix contains clusters of said TiB.sub.2 particles greater than 10 microns in size with an average of less than 4 of said clusters per 2 cm.sup.2. The alloy is prepared by adding a boron containing material selected from the group consisting of borax, boron oxide, boric acid and mixtures thereof, and K.sub.2 TiF.sub.6 to a bath of molten aluminum and stirring the molten mixture.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.