Patent · US Expired

Microwave dielectric ceramic composition

US5489559A · kind A · utility

0Cited by
4References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 23, 1994
Grant dateFeb 6, 1996
Priority date
Expiry dateDec 23, 2014

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/495
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

The present invention provides a microwave dielectric ceramic composition in which .epsilon.r, Qu and .tau.f are generally controlled within a practical characteristic range and each of the characteristics is maintained in a well balanced state. A ceramic composition of the present invention comprises a composition represented by xBi.sub.2 O.sub.3 -(1-x) (yNb.sub.2 O.sub.5 -(1-y)Ta.sub.2 O.sub.5) in which 0.45.ltoreq.x.ltoreq.0.55 and 0.1.ltoreq.y<1.0 as a main ingredient, to which not more than 0.8 parts by weight of V.sub.2 O.sub.5 is added and incorporated. An another ceramic composition comprises a composition represented by Bi(NbxTa1-x)O.sub.4 in which 0<x.ltoreq.0.96 as a main ingredient, to which not more than 5 wt % of V.sub.2 O.sub.5 and not more than 2 wt % of PbO are added and incorporated. An another ceramic composition comprises the main ingredient as described above to which not more than 5 wt % of V.sub.2 O.sub.5 and not more than 2 wt % of MnO.sub.2 are added and incorporated. An another ceramic composition comprises the main ingredient as described above to which not more than 2 wt % of V.sub.2 O.sub.5 and not more than 1 wt % of TiO.sub.2 are added and incorporate…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.