Patent · US Expired

Method to separate and recover resin and steel pipe from resin-coated steel pipe

US5512104A · kind A · utility

6Cited by
4References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 11, 1994
Grant dateApr 30, 1996
Priority date
Expiry dateMar 11, 2014

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB08B7/0071
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

In order to utilize separately steel pipe and coating resin as recycling resources, resin-coated steel pipe, which is produced by adhering a thermo-plastic coating resin on the surface of steel pipe with an adhesive, is heated by high-frequency induction heating to at least the melting temperature of the coating resin, and the coating resin is scraped off while the inner layer thereof is in a melted condition and the outer layer is in a softened condition. Coating resin and steel pipe can be recovered without the composition thereof being damaged. The scraping of coating resin is complete and efficient and requires only minimal energy since it occurs when the inner layer of the coating resin is in a melted condition and the outer layer is in a softened condition.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.