Method of manufacturing a composite
US5514453A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 6, 1995 |
| Grant date | May 7, 1996 |
| Priority date | — |
| Expiry date | Jun 6, 2015 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/2956
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The pyrolytic carbon lamellar interphase is formed on the reinforcing fibers inside a chamber in which a plurality of successive cycles is performed, each cycle comprising: injecting a reaction gas in which the pyrolytic carbon precursor is selected from alkanes, excluding methane taken as a sole component, alkenes, alkynes, and aromatic hydrocarbons, and mixtures thereof; the gas is maintained inside the chamber for a first predetermined time period to form an interphase layer of controlled thickness of nanometer size; the gaseous reaction products are then evacuated during a second time period; the cycles being performed consecutively in the chamber until the thickness desired for the interphase has been obtained, thereby achieving a lamellar interphase that is highly anisotropic, whose lattice fringe texture has distorted fringes of total length (L.sub.2) not less than 4 nanometers on average with maximum values exceeding 10 nanometers.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.