Method of annealing iron-based products comprised of carbon steel rich in chromium and manganese
US5536338A · kind A · utility
3Cited by
0References
6Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Dec 6, 1994 |
| Grant date | Jul 16, 1996 |
| Priority date | — |
| Expiry date | Dec 6, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D1/76
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of annealing of siderurgical products comprised of carbon steel having a chromium content in the range 0.15-1.5 wt. % and a manganese content also in the range 0.15-1.5 wt. %, whereby said products are held in an annealing furnace under nitrogen atmosphere to bring about globulization of the perlite; characterized in that oxygen is added to this atmosphere, in an amount greater than or equal to 0.5 vol. %.