Abstract
A TiAl base alloy containing 46 to 54 mol % of Ti and 46 to 52 mol % of Al in which Sb is added within a range of 0.1 to 1 mol %, at least one element of Hf and/or Zr is further added within a range of 0 to 3 mol %, and three phases of a .gamma. phase, an .alpha..sub.2 phase and Sb-rich phase coexist.