Cathode assembly incorporating a black layer formed from particles having a specified average particle size
US5543682A · kind A · utility
5Cited by
2References
3Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 17, 1994 |
| Grant date | Aug 6, 1996 |
| Priority date | — |
| Expiry date | Mar 17, 2014 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01J2209/012
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A black coating having a uniform thickness is formed, on the inner surface of the cathode sleeve, as a sintered layer obtained by mixing tungsten having an average particle diameter in a range of 0.5 .mu.m (inclusive) to 2 .mu.m (inclusive) with alumina having an average particle diameter in a range of 0.1 .mu.m (inclusive) to 1 .mu.m (exclusive) at a weight ratio of the tungsten to the alumina in a range of (90:10) to (65:35).