Copolymers and their use in the treatment of leather
US5556930A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 12, 1995 |
| Grant date | Sep 17, 1996 |
| Priority date | — |
| Expiry date | Jun 12, 2015 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC14C9/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention relates to copolymers built up of a) 20-60%-wt. ethylenically unsaturated acid-groups-comprising monomers, b) 40-80%-wt. ethylenically unsaturated glycerol derivatives in which one hydroxyl group of the glycerol is unsubstituted, one hydroxyl group is etherified with (meth)-allyl alcohol and the third hydroxyl group is etherified with a C.sub.12 -C.sub.24 -alcohol or C.sub.12 -C.sub.24 -alkyl phenol or esterified with a C.sub.12 -C.sub.40 -monocarboxylic acid and c) 0-30%-wt. other ethylenically unsaturated monomers copolymerizable with the monomers a) and b), whereby the sum of the monomers a+b+c=100. The present invention further relates to the use of said copolymers for the softening of leather. The copolymers according to the present invention result in an improved exhaustion during the leather treatment.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.