Patent · US Expired

Co-dried aluminum oxyhydroxides

US5558858A · kind A · utility

0Cited by
14References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 17, 1990
Grant dateSep 24, 1996
Priority date
Expiry dateSep 17, 2010

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01F7/02
  • WIPO fieldPharmaceuticals
  • WIPO sectorChemistry

Abstract

Adsorptive, protein-binding aluminum oxyhydroxides are prepared by mixing carbonate-free, highly hydrated, aluminum oxyhydroxide containing aqueous suspensions with water soluble additives that furnish coordinating moieties with the aluminum compound and drying the resultant mixture. The protein-binding aluminum oxyhydroxides can be made resuspendable by acidifying to a pH value of between about 4 and about 6.5. Such acidification can occur either before or after drying.