Method of producing a sintered carbonitride alloy for fine to medium milling

US5561831A · kind A · utility

0Cited by
10References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 11, 1995
Grant dateOct 1, 1996
Priority date
Expiry dateMay 11, 2015

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22F9/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

According to the invention there now is provided a method of producing a sintered titanium based carbonitride alloy with 3-25 weight-% binder phase with extremely good properties at fine to medium coarse milling. The method relates to the use of a raw material consisting of a complex cubic carbonitride comprising the main part of the metals from groups IV and V of the periodic system and carbon and nitrogen to be found in the finished alloy whereby said alloy has the composition PA1 0.89.ltoreq.X.sub.IV .ltoreq.0.97 PA1 0.52.ltoreq.X.sub.C .ltoreq.0.61 where X.sub.IV is the molar ratio of the group IV elements of the alloy and X.sub.C is the molar ratio of carbon.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.