Low solvent, thermoplastic polyurethane containing solvent cement
US5563193A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jan 25, 1996 |
| Grant date | Oct 8, 1996 |
| Priority date | — |
| Expiry date | Jan 25, 2016 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/3158
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
There is now provided a solvent cement having a total of less than 80 weight percent of solvents and a thermoplastic polyurethane elastomer as at least one of the resins dissolved in the solvent. The solvent mixture contains at least a 5- or 6-membered water miscible lactone or lactam such as N-methyl-2-pyrrolidone (NMP) in an amount of 21 weight percent or less based on the weight of all the ingredients. The reduced solvent concentration assists in lowering VOC emissions while preserving the hydrostatic burst strength mechanical property required by ASTM D 2564-88.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.