Patent · US Expired

High temperature stable continuous filament glass ceramic fibers

US5569629A · kind A · utility

44Cited by
19References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 6, 1995
Grant dateOct 29, 1996
Priority date
Expiry dateJun 6, 2015

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD04H1/4218
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Composition and process for the preparation of high temperature stable continuous glass ceramic fibers with an upper temperature use limit of 2300.degree. F. are provided. The compositional formulation, in mole percent, is 62-85% SiO.sub.2, 9.5-20% Al.sub.2 O.sub.3, 5-15.5% MgO, 0.5-5% TiO.sub.x, and 0-5% ZrO.sub.2. The continuous fibers are prepared by an economical direct melt method, and demonstrate high tensile strength, high Young's modulus, and low linear thermal shrinkage characteristics.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.