Patent · US Expired

Kaolin clay slurries having reduced viscosities and process for the manufacture thereof

US5593490A · kind A · utility

9Cited by
17References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 26, 1995
Grant dateJan 14, 1997
Priority date
Expiry dateJun 26, 2015

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/22
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A kaolin clay slurry having a reduced viscosity is manufactured by a process which comprises the sequential steps of mechanically working an undispersed crude kaolin clay material having a solids content of at least about 65 percent, by weight, under conditions which insure that the kaolin clay material will be subjected to an energy level of at least 10 horsepower-hours per ton of dry kaolin clay material and then subjecting the mechanically worked kaolin clay material to centrifugation to substantially remove any particles having a diameter less than about 0.2 microns.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.