Method for preparing elongated-shaped silica sol

US5597512A · kind A · utility

73Cited by
10References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 14, 1994
Grant dateJan 28, 1997
Priority date
Expiry dateOct 14, 2014

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB01J13/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for preparing a silica sol having an elongated shape comprising a step (a) where an aqueous solution containing a water-soluble calcium salt or a water-soluble magnesium salt or a mixture of the water-soluble calcium salt or the water-soluble magnesium salt is mixed with an aqueous colloidal solution of an active silicic acid; a step (b) where an alkaline substance is mixed with the aqueous liquid obtained in the step (a); a step (c) where a part or the whole of the mixture obtained in the step (b) is heated at 60.degree. C. or higher to obtain a heel solution and a feed solution is prepared by a part of the mixture obtained in the step (b) or a mixture separately prepared by the step (b) and the feed solution is added to the heel solution; and a step where water is evaporated during said addition step so that SiO.sub.2 concentration is concentrated to 6 to 30% by weight.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.