Patent · US Expired

Thermoplastic polyurethane elastomer based on a hydroxyl terminated polyol, an aromatic chain extender and 1,5 naphthalene diisocyanate

US5599874A · kind A · utility

12Cited by
4References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 13, 1995
Grant dateFeb 4, 1997
Priority date
Expiry dateJul 13, 2015

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/24994
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A thermoplastic polyurethane elastomeric seal composition comprising, by weight, about 90% to 99% thermoplastic polyurethane elastomer and about 1% to 10% fibers. Also, the thermoplastic polyurethane elastomer is derived from the reactants comprising: (i) a mixture of polyol and an aromatic chain extender in a molar ratio in the range of from about 40:60 to about 60:40 of butanediol glycol adipate to hydroquinone bis 2-hydroxyethyl ether, and (ii) 1,5 naphthalene diisocyanate present in a molar ratio in the range of about 50:50 to about 54.5:45.5 of 1,5 naphthalene diisocyanate to the said first mixture of polyol and an aromatic chain extender. After curing, the thermoplastic polyurethane elastomeric seal compound has outstanding wear resistance and low compression set. This thermoplastic polyurethane elastomeric seal compound is particularly useful in making shaft seals subject to high wear and high pressure, for use in hydraulic rams in earthmoving equipment.