Process for the production of a firmly adhering, moisture-proof coating of plastic on a substrate
US5618372A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 15, 1995 |
| Grant date | Apr 8, 1997 |
| Priority date | — |
| Expiry date | Nov 15, 2015 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC09D4/06
- WIPO fieldPharmaceuticals
- WIPO sectorChemistry
Abstract
A process for the production of a firmly adhering, moisture-proof coating of plastic on a substrate of metal, ceramic, glass, or polymer by the application of a liquid preparation containing water, solvent, a (meth)acrylate, and a reactive polymer and by solidifying this coating by heating it to a temperature above 100.degree. C. is described. A first preparation is applied to the substrate and at least partially dried; a second preparation is then applied to the partially dried first preparation and at least partially dried. Then the coating is heated to a temperature in the range of 150.degree.-400.degree. C. to solidify it. The first preparation contains: PA1 5-25 wt. % of an aqueous copolymer suspension, the copolymer consisting of a mixture of 40-80 wt. % of acrylonitrile and 60-20 wt. % of butyl acrylate; PA1 5-20 wt. % of water; PA1 35-75 wt. % of a polar solvent; and PA1 3-15 wt. % of a (meth)acrylate which is nonvolatile at temperatures of up to 250.degree. C., with the provision that the percentages always add up to 100%; and the second preparation contains: PA1 5-20 wt. % of a 40-90 wt. % solution of an isocyanate group-free polyurethane baking resin in solvent naphtha 1…
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.