Catalyst for hydrorefining
US5648311A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Aug 14, 1994 |
| Grant date | Jul 15, 1997 |
| Priority date | — |
| Expiry date | Aug 14, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC10G45/08
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
The invention relates to a catalytic hydrorefining of mixtures of hydrocarbons which contain hetero atoms such as nitrogen, sulphur, halogens and/or oxygen. The characterizing feature of the invention is that nickel or a nickel-molybdenum alloy containing more than 30% nickel, residue molybdenum, is thermally treated in an air atmosphere at temperatures of 400.degree. to 1200.degree. C. for a period of 0.25 to 10 hours, whereafter it is subjected to a hydrogen activation in the temperature range of 200.degree. to 600.degree. C.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.