Patent · US Expired

Impact modifier combination for aromatic polyesters

US5652306A · kind A · utility

23Cited by
5References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 27, 1996
Grant dateJul 29, 1997
Priority date
Expiry dateMar 27, 2016

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L51/04
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

An improved toughened blend of an aromatic polyester with from 5 to 20 phr of an impact modifier, which impact modifier is a blend of (a) 80 to 85 weight percent of a core/shell impact modifier having a polybutadiene core and at least one shell formed from methyl methacrylate and styrene; and (b) 15 to 20 weight percent of a linear copolymer which contains from 50 to 85 parts of units derived from ethylene, from 5 to 40 parts of units derived from (meth)acrylic esters, and from 2 to 10 parts of a copolymerizable monomer containing an epoxy group. The toughened blend exhibits higher impact strength than would be calculated for the blend using a linear relationship based on values of notched Izod for two blends, each containing only one of the impact modifiers at an equal use level.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.