Patent · US Expired

Low-odor, higher molecular weight polyether polyols, a process for producing them, and their use for the production of polymers, cosmetics and pharmaceutical products synthesized from polyether polyols

US5652319A · kind A · utility

0Cited by
3References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 13, 1996
Grant dateJul 29, 1997
Priority date
Expiry dateAug 13, 2016

Classification

  • Technology area (CPC A)Human Necessities
  • CPC primaryA61Q19/00
  • WIPO fieldPharmaceuticals
  • WIPO sectorChemistry

Abstract

Low-odor, higher molecular weight polyether polyols are produced by purifying the polyether polyols at temperatures of 110.degree. to 150.degree. C. and pressures of 10 to 70 hPa with the addition of 5 to 30% by weight of water, wherein the water is passed in finely divided form, with a droplet diameter of about 5 to 100 .mu., through the polyether polyols to be purified for a time of metered addition of 1 to 5 hours.