Process for preparing high vinyl polbutadiene rubber
US5654384A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Mar 27, 1996 |
| Grant date | Aug 5, 1997 |
| Priority date | — |
| Expiry date | Mar 27, 2016 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S152/905
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
This invention reveals a process for preparing high vinyl polybutadiene rubber which comprises polymerizing 1,3-butadiene monomer with a lithium initiator at a temperature which is within the range of about 5.degree. C. to about 100.degree. in the presence of a sodium alkoxide and a polar modifier, wherein the molar ratio of the sodium alkoxide to the polar modifier is within the range of about 0.1:1 to about 10:1; and wherein the molar ratio of the sodium alkoxide to the lithium initiator is within the range of about 0.05:1 to about 10:1.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.