Patent · US Expired

Polyurethane elastomers having improved green strength and demold time and polyoxyalkylene polyols suitable for their preparation

US5670601A · kind A · utility

28Cited by
15References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 15, 1995
Grant dateSep 23, 1997
Priority date
Expiry dateJun 15, 2015

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G2410/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Elastomers exhibiting decreased demold times and improved green strength are prepared by reacting a di- or polyisocyanate with a monodisperse polyoxypropylene diol having ultra-low unsaturation, and preferably prepared by the double metal cyanide.t-butyl alcohol catalyzed polymerization of propylene oxide. Further improved demold times and elevated elastomer physical properties are made possible by the use of multidisperse polyoxyalkylene polyether polyol blends having an overall unsaturation of less than 0.010 meq/g and a polydispersity of about 1.4 or greater.