Process for preparing 3,4-polyisoprene rubber
US5677402A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 24, 1996 |
| Grant date | Oct 14, 1997 |
| Priority date | — |
| Expiry date | Jul 24, 2016 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F136/06
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
This invention reveals an initiator system which is comprised of (a) a lithium initiator, (b) a sodium alkoxide and (c) a polar modifier; wherein the molar ratio of the sodium alkoxide to the lithium initiator is within the range of about 0.05:1 to about 3:1; and wherein the molar ratio of the polar modifier to the lithium initiator is within the range of about 0.25:1 to about 5:1. The subject invention also discloses a process for preparing 3,4-polyisoprene rubber which comprises polymerizing isoprene monomer with a lithium initiator at a temperature which is within the range of about 30.degree. C. to about 100.degree. C. in the presence of a sodium alkoxide and a polar modifier, wherein the molar ratio of the sodium alkoxide to the lithium initiator is within the range of about 0.05:1 to about 3:1; and wherein the molar ratio of the polar modifier to the lithium initiator is within the range of about 0.25:1 to about 5:1.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.