Polycarbonate moulding materials with improved toughness
US5679759A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 20, 1995 |
| Grant date | Oct 21, 1997 |
| Priority date | — |
| Expiry date | Sep 20, 2015 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L69/005
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Thermoplastic moulding materials containing PA0 A. 15 to 80 parts by weight of a thermoplastic polycarbonate or polyester carbonate, and PA0 B. 4 to 40 parts by weight of a graft polymer of PA1 B.1 20 to 60 weight % of one or more monomers on PA1 B.2 40 to 80 weight % of one or more graft bases having glass transition temperatures <0.degree. C., and PA0 C. 16 to 45 parts by weight of a thermoplastic, aromatic vinyl (co)polymer, wherein the graft base B.2 has an average particle size (d.sub.50 value) of 0.20 to 0.35 .mu.m and the weight ratio of components B:C is between 2:1 and 1:4.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.