Method for the preparation of ultrafine fibrous assembly having twisted morphology
US5705635A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 14, 1996 |
| Grant date | Jan 6, 1998 |
| Priority date | — |
| Expiry date | Nov 14, 2016 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC07H1/00
- WIPO fieldOrganic fine chemistry
- WIPO sectorChemistry
Abstract
When a saturated aqueous solution of a bolaform glycolipid represented by the general formula EQU G--NH--CO--(CH.sub.2).sub.n --CO--NH--G, in which G is a residue derived from a D- or L-glucopyranose by excepting the reduced-terminal hydroxyl group and the subscript n is 10, 12 or 14, at a high temperature, e.g., 90 .degree. C. or higher, is cooled at a controlled rate of 0.5 .degree. C./minute or lower, crystallite growth of the precipitates proceeds to form an ultrafine fibrous assembly of up to several hundreds .mu.m length having a twisted fibrous morphology of right- or left-hand screw. The twisted fibrous assembly thus obtained has usefulness as a functional material in the field of fine chemicals and in the fields of electronic and information technologies.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.