Gel formers having reduced gelling time and forming gels with improved melting resistance
US5709821A · kind A · utility
112Cited by
12References
10Claims
0Family size
Assignees
Inventors
Key dates
| Filing date | Jan 16, 1996 |
| Grant date | Jan 20, 1998 |
| Priority date | — |
| Expiry date | Jan 16, 2016 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S516/927
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Gel formers comprising acid aluminum phosphate and a reaction product of boric acid and an alkanolamine, and further comprising alkali metal compounds in the aluminum: alkali metal ratio of 1:1.3-2.5 require short gelling times, and form gels having improved melting resistance.