Method for treating electrolyte to remove Li.sub.2 O
US5711019A · kind A · utility
18Cited by
12References
16Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jan 31, 1996 |
| Grant date | Jan 20, 1998 |
| Priority date | — |
| Expiry date | Jan 31, 2016 |
Classification
- Technology area (CPC A)Human Necessities
- CPC primaryA62D2101/43
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of removing Li.sub.2 O present in an electrolyte predominantly of LiCl and KCl. The electrolyte is heated to a temperature not less than about 500.degree. C. and then Al is introduced into the electrolyte in an amount in excess of the stoichiometric amount needed to convert the Li.sub.2 O to a Li-Al alloy and lithium aluminate salt. The salt and aluminum are maintained in contact with agitation for a time sufficient to convert the Li.sub.2 O.