Abstract

The invention relates to polyketone yarns of which the maximum tangential modulus at an elongation of more than 0.2% is at least 10 N/tex which display both high strength and, if so desired, a high elongation at break. The quality number, which is measured on a single filament out of a bundle of at least about 30 filaments spun simultaneously through one spinneret and given as .sigma., .epsilon., is higher than 85 mN/tex, preferably higher than 100 mN/tex. The quality number of a yarn spun through one spinneret of one or more holes is higher than 110 mN/tex, preferably higher than 120 mN/tex. The yarns are manufactured by extruding a solution of a linear polymer of alternating ethylene and carbon monoxide units in a resorcinol-containing solvent, after which the solvent is removed with the aid of methanol as coagulant.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.