Patent · US Expired

Zirconia-alumina ceramic article

US5726110A · kind A · utility

5Cited by
8References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 6, 1997
Grant dateMar 10, 1998
Priority date
Expiry dateMar 6, 2017

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/119
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention is a ceramic article of magnesium-X silicate, wherein X represents lithium, sodium, potassium or other monovalent ion from about 0.1 to 2 weight percent, and yttria stabilized zirconia and alumina composite from about 99.9 to 98 weight percent wherein the yttria stabilized zirconia has a molar ratio of yttria to zirconia of from 0.5:99.5 to 5:95 and the alumina comprises from 0.1 to 50 percent of the yttria stabilized zirconia and alumina composite.