Patent · US Expired

Polyurethane elastomers having improved green strength and demold time, and polyoxyalkylene polyols suitable for their preparation

US5728745A · kind A · utility

15Cited by
18References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 19, 1996
Grant dateMar 17, 1998
Priority date
Expiry dateDec 19, 2016

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G2410/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Elastomers exhibiting decreased demold times and improved green strength are prepared by reacting a di- or polyisocyanate with a monodisperse polyoxypropylene diol having ultra-low unsaturation, and preferably prepared by the double metal cyanide.t-butyl alcohol catalyzed polymerization of propylene oxide. Further improved demold times and elevated elastomer physical properties are made possible bythe use of multidisperse polyoxyalkylene polyether polyol blends having an overall unsaturation of less than 0.010 meq/g and a polydispersity of about 1.4 or greater.