Abrasion resistant glass
US5741745A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Oct 8, 1996 |
| Grant date | Apr 21, 1998 |
| Priority date | — |
| Expiry date | Oct 8, 2016 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03C3/091
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Abrasion resistant glass, which consists essentially of the following components: ______________________________________ SiO.sub.2 75.5 to 85.5 (wt %), RO 1 to 8 (wt %), R'.sub.2 O 10 to 23.5 (wt %), RO + R'.sub.2 O 11 to 24.5 (wt %), Al.sub.2 O.sub.3 0 to 5 (wt %), ______________________________________ RO/R'.sub.2 O (weight ratio) at most 0.5, provided that R is at least one member selected from Mg and Ca, and R' is at least one member selected from Li, Na and K, and of which the density measured at room temperature is at most 2.41 g/cc.