Coating composition and articles prepared therewith
US5744243A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 10, 1996 |
| Grant date | Apr 28, 1998 |
| Priority date | — |
| Expiry date | Sep 10, 2016 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31938
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Describes a composition for producing durable coatings and a process for preparing a single-layer broad band antireflective coating on solid substrates, such as glass, ceramics, metals, and organic polymeric materials. The coating composition comprises, in combination, acid catalyzed hydrolysis and condensation products of water-silane monomer mixture and a film forming amount of a polymer having functional groups selected from amino, hydroxy and carboxy, hydroxy and amino, amino and carboxy, and amino, hydroxy and carboxy. The described process comprises applying the aforesaid coating composition (or an acid catalyzed sol-gel coating composition) substantially free of preformed oxide sol and water soluble metal salt to the surface of a solid substrate, curing the applied coating, and treating the cured coating with an aqueous electrolyte solution for a time sufficient to produce a coating having graded porosity which is antireflective over a broad band of the visible spectrum.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.