Aluminum alloy brazing material and brazing sheet adaptable for heat exchanges
US5744255A · kind A · utility
Assignees
Inventors
Key dates
| Filing date | Sep 3, 1996 |
| Grant date | Apr 28, 1998 |
| Priority date | — |
| Expiry date | Sep 3, 2016 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/12764
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
A typical aluminum alloy brazing material includesover 7.0 wt. % and not more than 12.0 wt. % of Si: over 0.1 wt. % and not more than 8.0 wt. % of Cu. over 0.05 wt. % and not more than 0.5 wt. % or Fe, further at least one kind selected from a group consisting of over 0.5 wt. % and not more than 5.5 wt. % of Zn. over 0.002 wt. % and not more than 0.3 wt % of In and over 0.002 wt. % and not more than 0.3 wt. % of Sn, and the balance of Al an inevitable impurities. A typical cladded aluminum alloy brazing sheet with a three-layer structure includes a brazing material, a core material comprising over 0.6 wt. % and not more than 2.5 wt. % of Si, over 0.5 wt. % and not more 2.5 wt. % of Cu, over 0.05 wt. % and not more than 2.0 wt. % of Mn, and the balance of Al and inevitable impurities, and a sacrificial material comprising at least one kind selected from a group consisting of over 0.5 wt. % and not more than 6.0 wt. % of Zn. over 0.002 wt. % and not more than 0.3 wt. % of In, and over 0.002 wt. % and not more than 0.3 wt. % of Sn, and the balance of Al and inevitable impurities, or comprises a core material cladded both sides thereof with the brazing material. By using the inventive …
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.