Patent · US Expired

Process of making a non-circular cross-sectional fiber

US5753166A · kind A · utility

14Cited by
6References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 21, 1996
Grant dateMay 19, 1998
Priority date
Expiry dateOct 21, 2016

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD01F6/92
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

A melt extrusion composition made by combining about 99.9 to about 98.5 weight percent of at least one polyester and about 0.1 to about 1.5 weight percent additive provides for a polyester or copolyester non-circular cross-sectional fiber having at least four percent improved shape retention as compared to the same fiber made from a melt extrusion composition without the additive. The additive is present at the air-polymer interfacial surface during melt spinning. A method of making the fiber is also disclosed.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.