Patent · US Expired

Austenitic stainless steel for use when hot

US5753178A · kind A · utility

2Cited by
2References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 8, 1996
Grant dateMay 19, 1998
Priority date
Expiry dateAug 8, 2016

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/50
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Austenitic stainless steel for use when hot, the chemical composition of which, by weight, includes from 16% to 25% of Ni, from 16% to 18.5% of Cr, from 0% to 3% of Mo, from 0% to 2% of Mn, from 1% to 3.5% of Ti, from 0% to 1.5% of Al, less than 0.1% of C+N, up to 0.025% of B, the remainder being iron and impurities resulting from the production; the chemical composition additionally satisfying the relations: PA0 (0.94.times.Ni-65.times.F)/(1-F).gtoreq.12 and PA0 17.ltoreq.(1.07.times.Cr-1.5.times.F)/(1-F).ltoreq.22 with: PA0 F=0.0444.times.Ti+0.0777.times.Al-0.0592.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.