Regeneration of plastic diaphragm
US5755951A · kind A · utility
2Cited by
8References
19Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 16, 1997 |
| Grant date | May 26, 1998 |
| Priority date | — |
| Expiry date | Jun 16, 2017 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC25B15/00
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A process for the regeneration of plastic diaphragms is described, in which a mineral acid solution is mixed with a suitable corrosion inhibitor, this mixture is temperature controlled at from approximately 0.degree. to 100.degree. C., preferably 40.degree. to 80.degree. C., in particular 50.degree. to 70.degree. C., and passed through the diaphragm for from approximately 0.1 to 84 hours, preferably 1 to 72 hours, in particular 2 to 24 hours.