Patent · US Expired

Iron-nickel alloy for stretched shadow mask

US5788783A · kind A · utility

6Cited by
5References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 18, 1996
Grant dateAug 4, 1998
Priority date
Expiry dateJul 18, 2016

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C19/03
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An iron-nickel alloy useful for the manufacture of a stretched shadow mask, the chemical composition of the iron-nickel alloy containing by weight: 69%.ltoreq.Ni.ltoreq.83%, 0%.ltoreq.Mo.ltoreq.7%, 0%.ltoreq.Cu.ltoreq.8%, 0%.ltoreq.Co.ltoreq.1.5%, 0%.ltoreq.W.ltoreq.7%, 0%.ltoreq.Nb.ltoreq.7%, 0%.ltoreq.V.ltoreq.7%, 0%.ltoreq.Cr.ltoreq.7%, 0%.ltoreq.Ta.ltoreq.7%, 0%.ltoreq.C.ltoreq.0.1%, 0%.ltoreq.Mn.ltoreq.1%, 0%.ltoreq.Si.ltoreq.1%, 0%.ltoreq.Ti.ltoreq.1.2%, 0%.ltoreq.Al.ltoreq.1.2%, 0%.ltoreq.Zr.ltoreq.1.2%, 0%.ltoreq.Hf.ltoreq.1.2%, S.ltoreq.0.010% the balance being iron and impurities resulting from smelting, the chemical composition furthermore satisfying the relationships: PA1 Co+ni+1.5.times.Cu.gtoreq.79.5%; 3.times.(Co+Ni)-2.times.Cu.gtoreq.206%; Co+Ni+7.times.Cu.ltoreq.130%; 7.times.(Co+Ni)+2.times.Cu.ltoreq.581%; Mo+W+Nb+V+Cr+Ta.ltoreq.7%; Ti+al+Zr+Hf.ltoreq.1.2%; C+Mn+Si.ltoreq.1%; 80.5.ltoreq.Co+Ni+0.80.times.Cu.ltoreq.81.7%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.