Corrosion and wear-resistant chill casting

US5795540A · kind A · utility

7Cited by
3References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 17, 1996
Grant dateAug 18, 1998
Priority date
Expiry dateSep 17, 2016

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C37/08
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A corrosion and wear-resistant chill cast part is formed from an iron composition comprising from 26 to 36 percent Cr; 0 to 10 percent Ni; 2 to 6 percent Mo; 0 to 3 percent Cu; 0 to 0.2 percent N; 0 to 1.5 percent Si; 0 to 1.5 percent Mn; 4 to 9 percent V; and 1.4 to 1.9 percent C. All percents are by weight of the total composition. The remainder of the composition is Fe and impurities.