Abstract
A method for manufacturing a mineral fiber panel which comprises uniformly dispersing in water 60 to 90% by weight of a mineral fiber, 2 to 19% by weight of an organic binder, 1 to 20% by weight of an inorganic microfiber, 0.5 to 3% by weight of a flocculant and 0.5 to 10% by weight of a thermally expansible resin fine particle which has a diameter after expansion of not less than 0.03 mm but less than 3.0 mm, the expansion degree of the above diameter being at least 3 times, and which has an expansion-starting temperature of 50.degree. to 105.degree. C., as the composition components, to prepare a slurry, and thereafter subjecting the slurry to wet forming and then to drying. The above production process enables the enhancement of productivity and the mineral fiber panel obtained by the above production process is light in weight and excellent in sound-absorbing qualities and fireproof properties.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.