Hardening composition and hardened product

US5810922A · kind A · utility

8Cited by
4References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 11, 1997
Grant dateSep 22, 1998
Priority date
Expiry dateApr 11, 2017

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02W30/91
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention is directed to a hardening composition characterized by comprising (A) a slag composition containing 0 to 37 wt. % of CaO, 23 to 90 wt. % of SiO.sub.2, and 0 to 40 wt. % of Al.sub.2 O.sub.3 and 0.1 to 50 wt. % of one or more compounds selected from the group consisting of iron oxide, alkali components, phosphorous components, titanium dioxide, manganese oxide, and magnesium oxide, and/or 0.1 to 10 wt. % of a halogen; and (B) an alkaline activator. The invention is also directed to a hardened product obtained by mixing the hardening composition with water. The properties of the hardened product are suitable for use as various concrete materials, and therefore, refuse-incinerated ashes sewage sludge, etc. are effectively utilized and recycled as a resource.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.