Abstract
Fine-grained kaolin clays having improved brightness can be produced by (a) using centrifugation to fractionate the clay starting material into finer and coarser fractions, (b) subjecting the coarser fraction to flotation to remove discoloring impurities and (c) combining the finer and floated coarser fractions to produce fine-grained kaolin clays having improved brightness.