Iron-based soft magnetic alloy containing cobalt for use as a solenoid core
US5817191A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Aug 26, 1997 |
| Grant date | Oct 6, 1998 |
| Priority date | — |
| Expiry date | Aug 26, 2017 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01F1/147
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
An iron-based, cobalt-containing soft magnetic alloy suitable for use as a core in a magnetic switch or other exciting circuits has a cobalt content of 6 through 30 weight percent, at least one of the elements chromium, molybdenum, vanadium and tungsten in range of 3 through 8 weight percent, and a remainder iron, possibly including inconsequential contaminants. The alloy has a coercive field strength of lower than or equal to 3.2 A/cm, and a saturation flux density of greater than 1.9 Tesla.