Sintered friction material, composite copper alloy powder used therefor and manufacturing method thereof

US5824923A · kind A · utility

32Cited by
3References
39Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 28, 1995
Grant dateOct 20, 1998
Priority date
Expiry dateSep 28, 2015

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22F2999/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A sintered friction material includes a copper alloy base and hard particles. The copper alloy base includes copper and at least one of, and preferably both, Zn and Ni within a total range of 5 to 40 wt % of the copper alloy base. The hard particles are uniformly dispersed in a matrix formed by the original composite copper alloy powder constituting the base, in a content amount within a range of 10 to 30 wt % of the friction material.