Patent · US Expired

Method for electrically coloring aluminum material and gray-colored aluminum material obtained thereby

US5849169A · kind A · utility

1Cited by
6References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 18, 1997
Grant dateDec 15, 1998
Priority date
Expiry dateNov 18, 2017

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC25D11/22
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

Disclosed are a method for electrolytically coloring an aluminum material which is capable of coloring an anodic oxide film in a gray color and a gray-colored aluminum material obtained thereby. In a method for electrolytically coloring an aluminum material having the anodic oxide film formed on the surface thereof in an electrolytic coloring solution containing an inorganic metal salt, a strongly acidic electrolytic coloring solution containing sulfuric acid, stannous sulfate, nickel sulfate, and ammonium sulfate and having a pH of not more than 2.5 is used as the electrolytic coloring solution. Preferably the electrolytic coloring solution contains sulfuric acid at a concentration in the range of 3 to 30 g/liter, stannous sulfate at a concentration in the range of 0.1 to 3.0 g/liter, nickel sulfate at a concentration in the range of 10 to 100 g/liter, and ammonium sulfate at a concentration in the range of 20 to 100 g/liter. By this method, a gray-colored aluminum material possessed of an anodic oxide film colored in an achromatic or substantially achromatic gray color is obtained.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.