Method for manufacturing a friction-wear aluminum part
US5884388A · kind A · utility
27Cited by
8References
22Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | May 20, 1997 |
| Grant date | Mar 23, 1999 |
| Priority date | — |
| Expiry date | May 20, 2017 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T29/49984
- WIPO fieldMechanical elements
- WIPO sectorMechanical engineering
Abstract
A friction-wear aluminum part which includes a metal substrate and friction-wear coating applied to at least a portion of the outer surface to said substrate. The coating is a mixture of both aluminum and stainless steel. On a preferred basis, the surface of the substrate is intentionally roughened or grooved to facilitate bonding of the coating thereto. An associated method is also disclosed.