High strength steel is produced by a first rolling of a steel composition, reheated above 1100.degree. C., above the austenite recrystallization, a second rolling below the austenite recrystallization temperature, water cooling from above AR.sub.3 to less than 400.degree. C. and followed by tempering below the Ac.sub.1 transformation point.